Wear-resistant and available in a wide Variety

ZetaBeads® Plus are yttrium-stabilized high-end zirconium oxide grinding media of a high density and hardness. In addition, the very good sphericity and polished surface of the grinding beads contribute to an extremely high wear-resistance which prevents product contamination. ZetaBeads® Plus grinding balls are ideal for dispersion processes and true comminution of high-quality products.

Available standard qualities

TypeFraction [mm]
ZetaBeads® Plus 0.07

0.07 - 0.12

ZetaBeads® Plus 0.1

0.1 - 0.2

ZetaBeads® Plus 0.2

0.2 - 0.3

ZetaBeads® Plus 0.3

0.3 - 0.4

ZetaBeads® Plus 0.38

0.38 - 0.42

ZetaBeads® Plus 0.4

0.4 - 0.5

ZetaBeads® Plus 0.5

0.5 - 0.6

ZetaBeads® Plus 0.6

0.6 - 0.7

ZetaBeads® Plus 0.8

0.7 - 0.9

ZetaBeads® Plus 0.9

0.8 - 1.0

ZetaBeads® Plus 1.0

0.9 - 1.2

ZetaBeads® Plus 1.3

1.2 - 1.5

ZetaBeads® Plus 1.7

1.5 - 2.0

ZetaBeads® Plus 2.2

2.0 - 2.5

ZetaBeads® Plus 3.0

2.6 - 3.3

Chemical composition

about (in weight %) 
ZrO2 + HfO2

94

Y2O3

5

Others

< 1

Mechanical properties

  
Densitiy

6.0 kg/l

Bulk density

~ 3.6 kg/l

Vickers hardness

> 1150 HV

Young modulus> 200 GPa

You can purchase ZetaBeads® Plus in our Customer Portal

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

you may also be interested in:

AI Overview
An error occurred. Please try again.