High-purity yttrium-stabilized zirconium oxide grinding beads for precision nano wet grinding and dispersion applications.
NETZSCH-Beads®

ZetaBeads® Nano

Wear-resistant with extremely small Diameters 

ZetaBeads® Nano are made of yttrium-stabilized, high-purity zirconium oxide powder. Thanks to their high density and extreme hardness, product contamination is avoided. With diameters ranging from 30 μm to 200 μm, ZetaBeads® Nano are particularly suitable for dispersion and wet grinding of high-tech products down to the lower nanometer range.

Available standard qualities

TypeØ [mm]
ZetaBeads® Nano 0.03

0.015 - 0.05

ZetaBeads® Nano 0.05

0.03 - 0.08

ZetaBeads® Nano 0.1

0.08 - 0.13

ZetaBeads® Nano 0.2

0.17 - 0.27

Chemical composition

about (in weight %) 
ZrO2 + HfO2

95

Y2O3

5

Mechanical properties

  
Densitiy

6.0 kg/l

Bulk density

~ 3.6 kg/l

Vickers hardness

> 1200 HV

Young modulus> 200 GPa

You can purchase ZetaBeads® Nano in our Customer Portal

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

you may also be interested in:

AI Overview
An error occurred. Please try again.