Small yellow grinding beads scattered on a clean white surface representing NETZSCH CeraBeads for iron-free dispersing applications.
NETZSCH-Beads®

CeraBeads

Wear-resistant and Iron-free

CeraBeads are cerium-stabilized zirconium oxide grinding media of a high density and hardness. They are suitable for a wide variety of applications that require iron-free processing. CeraBeads optimize your costs and deliver very high grinding efficiency.

Available standard qualities

TypeFraction [mm]
CeraBeads 0.3

0.3 - 0.4

CeraBeads 0.4

0.4 - 0.6

CeraBeads 0.6

0.6 - 0.8

CeraBeads 1.0

0.9 - 1.1

CeraBeads 1.2

1.2 - 1.4

CeraBeads 1.4

1.4 - 1.6

CeraBeads 1.6

1.6 - 1.8

CeraBeads 1.8

1.8 - 2.0

CeraBeads 2.0

2.0 - 2.2

CeraBeads 2.5

2.3 - 2.7

CeraBeads 3.0

2.6 - 3.3

Chemical composition

about (in weight %) 
ZrO2

82

CeO2

16

Others

2

Mechanical properties

  
Densitiy

6.2 kg/l

Bulk density

~ 3.8 kg/l

Vickers hardness

> 1180 HV

You can purchase CeraBeads in our Customer Portal

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

you may also be interested in:

AI Overview
An error occurred. Please try again.