NETZSCH-Beads®

SteelBeads Q

High material density, also for applications in the foods industry

SteelBeads Q are food grade chromium steel grinding media, W 1.3505, with a very good sphericity. The high density of 7.85 kg/l enables the dispersion of high-viscosity products. SteelBeads Q are available in a range of 2 mm to 8 mm in diameter.

Available standard qualities

TypeØ [mm]
SteelBeads Q 2

2.0

SteelBeads Q 3

3.0

SteelBeads Q 4

4.0

SteelBeads Q 5

4.8

SteelBeads Q 6

6.35

SteelBeads Q 8

8.0

Chemical composition

Elementweight %
C

1

Mn

0.3

P

-

S

-

Si

0.2

Cr

1.4

Ni

-

Cu

-

Fe

rest

Mechanical properties

  
Densitiy

7.85 kg/l

Bulk density

~ 4.8 kg/l

Rockwell

60 - 66 RW