Toll Grinding

Screening / Classifying

NETZSCH Screening/Classifying

A customized solution, even for the trickiest separation tasks: NETZSCH offers a broad range of systems and technologies for separation. Our screening machines are used primarily for separating oversize particles from special-effect pigments. The dynamic air classifiers master extreme demands – such as abrasive or high-purity products – with the highest degree of separation.

Performance

  • Materials with a Mohs hardness up to 10
  • Charge range: < 0.02 mm to < 10 mm
  • Fineness range: 3 µm to 0.3 mm
  • Output range: up to 10,000 t/year

Specialization

  • Iron particle-free separation of coarse material
  • Processing of products with high adhesion and coating behavior
  • Dynamic air classifier achieves the finest and cleanest upper grain boundaries

Equipment

  • Screening machines
  • Dynamic air classifiers

Tailored Toll Processing

Precision and quality for your products.

Contact us

Product examples

ProductProcessFineness (µm)
Baritescreening / classificationd50 1.1
Calcium hydroxidescreening / classificationd50 2.3
Epoxy resinfine grinding - dry / screeningd50 27.1
Pea flourscreening / classificationd50 10.7
Glass fritsfine grinding - dry / screeningd50 3.3
Graphitefine grinding - dry / screeningd50 4.8
Silicafine grinding - dry / screeningd50 3.6
Tonerfine grinding - dry / screeningd50 7.1
Cementscreening / classificationd50 2.4