A customized solution, even for the trickiest separation tasks: NETZSCH offers a broad range of systems and technologies for separation. Our screening machines are used primarily for separating oversize particles from special-effect pigments. The dynamic air classifiers master extreme demands – such as abrasive or high-purity products – with the highest degree of separation.
Performance
- Materials with a Mohs hardness up to 10
- Charge range: < 0.02 mm to < 10 mm
- Fineness range: 3 µm to 0.3 mm
- Output range: up to 10,000 t/year
Specialization
- Iron particle-free separation of coarse material
- Processing of products with high adhesion and coating behavior
- Dynamic air classifier achieves the finest and cleanest upper grain boundaries
Equipment
- Screening machines
- Dynamic air classifiers

Tailored Toll Processing
Product examples
Product | Process | Fineness (µm) |
---|---|---|
Barite | screening / classification | d50 1.1 |
Calcium hydroxide | screening / classification | d50 2.3 |
Epoxy resin | fine grinding - dry / screening | d50 27.1 |
Pea flour | screening / classification | d50 10.7 |
Glass frits | fine grinding - dry / screening | d50 3.3 |
Graphite | fine grinding - dry / screening | d50 4.8 |
Silica | fine grinding - dry / screening | d50 3.6 |
Toner | fine grinding - dry / screening | d50 7.1 |
Cement | screening / classification | d50 2.4 |