26.08.2016

서브미크론 범위의 건식 최고급 연삭 - 처리량 5배 증가

습식이든 건식이든 모든 분쇄 공정에서 미세 입자는 재응집되는 경향이 있습니다. 이러한 경향은 입자가 미세해질수록 증가합니다.

건식 입자 분쇄를 위해 설계된 NETZSCH 유동층 제트 밀은 처리량과 효율성을 향상시키는 첨단 기술을 갖추고 있습니다.

During dry-grinding this formation of agglomerates causes a decrease in throughput capacity and reduces the process efficiency. The classifier in a fluidized bed jet mill cannot discern individual fine particles, but rather recognizes the agglomerate as one large particle which is then reintroduced into the grinding process. In a closed system such as a fluidized bed jet mill, the agglomerates thus remain in the mill, ostensibly to be ground even finer.

Prevention of Reagglomeration

In particular for the NETZSCH s-Jet®® process by NETZSCH Trockenmahltechnik, in which steam is used as a grinding medium instead of air to give higher capacities and to open up new ranges of fineness (submicron) for the dry-grinding sector, the stabilization of the finest particles produced is of great importance. This is done by adding suitable dispersing agents. If the amount of dispersing agent added is approx. 0.1 to 1 %, this decreases the electrostatic surface charge thus reducing reagglomeration. Depending on the product and additive used, the result is not just a fivefold increase in throughput, but also an improvement of the flowability, an increase in the surface area and a reduction of product deposits in the mill.

Use of Dispersing Agents

In the NETZSCH s-Jet®® process dispersing agents can be added in solid or liquid form. Solid agents are fed directly into the feed product via a dosing device whereas liquid agents are usually added via a dosing pump directly into the fluidized bed jet mill.

 

AI Overview
An error occurred. Please try again.