02.08.2021
셀브에 위치한 NETZSCH-Feinmahltechnik GmbH의 새로운 물류 센터 기공식
NETZSCH는 연삭 및 분산 사업부의 새로운 물류 센터에 600만 유로를 투자하고 혁신과 새로운 프로세스를 통해 치열한 국제 경쟁에 대응하고자 합니다. 보다 효율적인 프로세스와 프로젝트별 기계 디지털화를 통해 사업부는 이제 고객이 적시에 적재적소에 올바른 부품을 공급할 수 있도록 지원할 수 있게 되었습니다.

The final assembly of machines and systems is already located in a 7,500 m2 production hall on the grounds of NETZSCH-Feinmahltechnik GmbH in Selb, Breslauer Straße.
The Logistics Center serves, on the one hand, to increase the efficiency of final assembly and, on the other hand, to relieve the production facility in Tirschenreuth with respect to space and capacity.
The logistics center will be a single-story hall with an upstream incoming/outgoing goods zone. Offices for loading supervisors and logistics processing will be integrated into the building.
Due to the vastly different dimensions and weights of the components, a wide variety of logistics systems will be used in the hall. Around 30 employees will use approx. 85% of the space for warehouse logistics. About 15% of the area will be used for the assembly of small components, packaging and goods issue.
Cornerstones of our new Logistics Center:
- Dimensions: 36 m x 90 m
- Height: approx. 11 m
- Floor area: approx. 3,200 m²
- Reinforced concrete skeleton construction with insulated metal façade
- Open to daylight via skylight dome and window strips
- High insulation standard and highly efficient, gas-fired dark radiator heating system
- Total investment: around € 6 million
- Planned completion of construction: beginning of 2022