Toll Grinding

Micronization / Comminution

NETZSCH Micronization/Comminution

NETZSCH Lohnmahltechnik is the specialist for high-quality, abrasion-free dry grinding in the micron and nano range. From a few hundred grams, which we process in our pilot-plant machines, through to industrial quantities of several tons per hour - we have the equipment that is ideally suited for the desired optimization of your product – naturally in combined processes, such as simultaneous grinding and coating of particles, as well. Talk to us!

Performance

  • Materials with a Mohs hardness up to 10
  • Charge range: < 2 mm to 500 mm
  • Fineness range: 2 µm to 10 mm
  • Output range: up to 20,000 t/year

Specialization

  • Both iron-free and contamination-free micronization
  • Toll grinding of small batches
  • Use of our opposed jet mill for micronization into the nano range
  • Grinding with additives
  • Plastic or ceramic lining of components
  • Pressure-shock resistant
  • Cold grinding, hot gas grinding and steam jet grinding

Equipment

  • Broyeurs à marteaux
  • Concasseurs à mâchoires
  • Broyeurs à rouleaux
  • Broyeurs à jet d'impact
  • Broyeurs à jet opposé
  • Broyeurs à billes (en discontinu)
  • Broyeurs classificateurs

Traitement personnalisé des péages

Précision et qualité pour vos produits.

Contactez nous

Product examples

ProductProcessFineness (µm)
Aluminum oxidefine grinding - dryd50 1.3
Boron carbidefine grinding - dryd50 1.7
Calcium phosphatefine grinding - dryd50 20
Sodium sulfatefine grinding - dryd50 1.4
Pigmentfine grinding - dryd50 1.2
Powder coatingfine grinding - dryd50 0.7
Silicon carbidefine grinding - dry / classifyingd50 1.2
Tonerfine grinding - dry / classifyingd50 7.1
Cellulosefine grinding - dry> 100

Our Technologies and Contact Persons at the Locations:

Le siège de NETZSCH à Bobingen, avec une architecture moderne aux accents rouges et des bannières d'entreprise sur fond de ciel bleu.
Broyage à sec et classification à Bobingen / Allemagne

Bobingen is the location of the NETZSCH Lohnmahltechnik GmbH headquarters. Here we offer micronization of dry materials into the nanometer range.

Le siège de NETZSCH à Bobingen, un bâtiment en briques distinctif, comporte des drapeaux et une entrée spacieuse, idéale pour les services de broyage à façon.
Broyage à sec et classification à Hanau / Allemagne

Our facility in Hanau specializes in micronization and the classification of dry materials. It is located directly in the Wolfgang Industrial Park.

Vue aérienne de l'usine NETZSCH entourée de verdure, présentant les capacités de micronisation avancées pour les matériaux secs.
Broyage humide et sec à Pomerode / Brésil

Notre service Toll Grinding comprend également des solutions telles que le remplissage et l'étiquetage. Grâce à une technologie de pointe, à un contrôle de qualité strict et à l'expertise de nos spécialistes, nous garantissons des processus personnalisés, efficaces et flexibles, depuis les essais en laboratoire jusqu'à la production à grande échelle.