NETZSCH Lohnmahltechnik is the specialist for high-quality, abrasion-free dry grinding in the micron and nano range. From a few hundred grams, which we process in our pilot-plant machines, through to industrial quantities of several tons per hour - we have the equipment that is ideally suited for the desired optimization of your product – naturally in combined processes, such as simultaneous grinding and coating of particles, as well. Talk to us!
Performance
- Materials with a Mohs hardness up to 10
- Charge range: < 2 mm to 500 mm
- Fineness range: 2 µm to 10 mm
- Output range: up to 20,000 t/year
Specialization
- Both iron-free and contamination-free micronization
- Toll grinding of small batches
- Use of our opposed jet mill for micronization into the nano range
- Grinding with additives
- Plastic or ceramic lining of components
- Pressure-shock resistant
- Cold grinding, hot gas grinding and steam jet grinding
Equipment
- Molinos de martillos
- Trituradoras de mandíbulas
- Trituradoras de rodillos
- Molinos de chorro de impacto
- Molinos de chorro opuesto
- Molinos de bolas (discontinuos)
- Molinos clasificadores
Product examples
| Product | Process | Fineness (µm) |
|---|---|---|
| Aluminum oxide | fine grinding - dry | d50 1.3 |
| Boron carbide | fine grinding - dry | d50 1.7 |
| Calcium phosphate | fine grinding - dry | d50 20 |
| Sodium sulfate | fine grinding - dry | d50 1.4 |
| Pigment | fine grinding - dry | d50 1.2 |
| Powder coating | fine grinding - dry | d50 0.7 |
| Silicon carbide | fine grinding - dry / classifying | d50 1.2 |
| Toner | fine grinding - dry / classifying | d50 7.1 |
| Cellulose | fine grinding - dry | > 100 |
Literatura de aplicación
Our Technologies and Contact Persons at the Locations:

Bobingen is the location of the NETZSCH Lohnmahltechnik GmbH headquarters. Here we offer micronization of dry materials into the nanometer range.

Our facility in Hanau specializes in micronization and the classification of dry materials. It is located directly in the Wolfgang Industrial Park.

Nuestro servicio de Toll Grinding también incluye soluciones como el llenado y el etiquetado. Con tecnología avanzada, un estricto control de calidad y la experiencia de nuestros especialistas, garantizamos procesos personalizados, eficientes y flexibles, desde las pruebas de laboratorio hasta la producción a gran escala.