Stress Number
The stress number indicates how often a single particle is theoretically stressed in a grinding chamber or stress zone. Similar to the stress energy, the stress number is subject to a stress number distribution.
Optimum comminution or dispersion results are achieved by optimizing the stress energy while maximizing the stress number.