Baterias
Materiais de Ânodo e Cátodo
One option for the synthesis of cathode and anode materials is the so-called solid-state process. In this process route, the active material is created from the raw materials through a chemical transformation in suitable furnaces. Depending on the raw materials used, a wet grinding stage with dry pre-grinding processes can be required for the raw materials prior to the synthesis.
The CGS and s-Jet® fluidized bed jet mills can be used for the dry grinding. For the wet grinding, the Zeta®, Neos or Zeta® RS agitator bead mills are used, depending on the required target fineness. Synthesis via a furnace process can result in the formation of undesired agglomerates. In order to separate these, a dry dispersion with a CSM classifier mill is usually carried out after the synthesis furnace, without change of the original size and shape of primary particles.

Os compostos típicos para materiais de cátodo são:
- LCO (óxido de lítio e cobalto, LiCoO2)
- NCA (óxido de lítio-níquel-cobalto-alumínio, LiNiCoAlO2)
- NMC (óxido de lítio-níquel-manganês-cobalto, Li[NiCoMn]O2)
- LMO (óxido de lítio-manganês, LiMn2O4)
- LFP (fosfato de ferro e lítio, LiFePO4)
- A folha condutora é geralmente feita de alumínio
Alguns exemplos de materiais ativos para ânodos são:
- Carbono amorfo
- Grafite
- Titanato de lítio (LTO, Li4Ti5O12)
- Materiais metálicos para ânodos (silício, estanho)
- A folha condutora é geralmente feita de cobre.
Wet Grinding
Products & Solutions in the field of Wet Grinding
Dry Grinding
Products & Solutions in the field of Dry Grinding
Mistura