Agglomerates, Aggregates, 
Primary particles

Agglomerates are clusters of aggregates and/or primary particles in a relatively loose punctual compound that are essentially held together by particle interactions.

图示显示了四种类型的颗粒:绿色团聚体、红色聚集体、黑色原生颗粒和浅灰色聚集颗粒。

Aggregates have a flat, form-fitting composite of primary particles or crystallites or even solid bridges between the individual primary particles.

团聚体、聚集体和原生颗粒的图示,突出了它们的不同结构和关系。

Primary particles are clearly differentiated crystalline or amorphous particles, which are not be interrupted by fractures.

代表不同粒子类型的彩色几何图形:绿色立方体、红色球体、灰色圆柱体和纹理粒子群。