are special designs of agitator bead mills and are among the slow-running mills with circumferential speeds of approx. 0.5 m/s -2 m/s. Some of them are still used today for the comminution of abrasive hard materials such as silicon carbide.

Attritor 磨机的详细示意图,展示了其用于研磨碳化硅等硬质材料的搅拌器设计。
根据 Klein 和 Szegvari(1928 年),Attritor Mill


In the case of continuously operated horizontally arranged agitator bead mills, the product suspension is pumped into the grinding vessel at the front via the product inlet.

NETZSCH Attritor 磨机展示了研磨室、产品入口和分离系统等关键部件,旨在实现高效研磨。

The agitator is located in the grinding chamber. In this case, agitating elements in the form of solid discs, perforated discs, pins, pegs or other elements are generally arranged on an a agitator shaft. The agitator shaft is operated at circumferential speeds of up to 20 m/s.  

Attritor 磨机各种搅拌器元件的技术图解,展示了实现最佳研磨效率的设计方案。

The grinding chamber is usually filled with 70 - 90 % bulk volume with grinding media. The product suspension leaves the grinding chamber via a grinding media separator. This can be designed as a friction gap or as a screen cartridge, for example. In order to cool the machine, the grinding vessels are usually double-walled.

图解说明了 Attritor 磨机的各种研磨介质分离方法,突出了其独特的设计。

At NETZSCH-Feinmahltechnik GmbH, the development led to the development of different grinding chamber and agitator shaft geometries, which are suitable for a wide variety of applications depending on the properties of the product suspensions and the product and quality requirements.