Давальческий помол
Жидкое измельчение

With the most advanced grinding technology, you will achieve the grinding or dispersion of your products into the micron or nanometer range. Here you profit from the know-how of one the world's market leaders in the area of wet grinding!
Performance
- Materials with a Mohs hardness up to 10
- Charge range: < 0.02 mm to < 1 mm
- Fineness range: 50 nm to 0.3 mm
- Output range: up to 1000 t/year
Specialization
- Both iron-free and contamination-free micronization
- Toll grinding of small batches
- Use of our Zeta® RS nano mill for finenesses into the nano range
- Plastic or ceramic lining of product-leading parts
- Explosion-protected ATEX zone
Equipment
- Many different types of agitator bead mills with various grinding systems
Product examples
| Product | Process | Fineness (µm) |
|---|---|---|
| Seaweed meal | Fine grinding - wet | d90 7.3 |
| UV absorber | Fine grinding - wet | d90 0.2 |
| Glass frits | Fine grinding - wet | d90 1 |
| Titanium oxide | Fine grinding - wet | d90 0.2 |
| Pigment paste | Fine grinding - wet | d90 0.9 |
| Aluminum oxide | Fine grinding - wet | d90 0.3 |
| Fertilizers | Fine grinding - wet | d90 4.4 |
| Calcium carbonate | Fine grinding - wet | d90 3.1 |
| Manganese oxide | Fine grinding - wet | d90 1.6 |
Наши технологии и контактные лица в филиалах:

Жидкое измельчение в Зельбе / Германия
Наши специалисты по жидкому измельчению находятся в Зельбе, где для вашего продукта имеется широкий ассортимент мельниц, смесителей и деаэраторов.

Жидкое и сухое измельчение в Помероде / Бразилия
Наши услуги контрактного измельчения также включают такие решения, как фасовка и маркировка. Благодаря передовым технологиям, строгому контролю качества и опыту наших специалистов мы обеспечиваем индивидуальные, эффективные и гибкие процессы - от лабораторных испытаний до полномасштабного производства.