ZsBeads are sintered zirconium silicate grinding beads with a high sphericity. In contrast to grinding beads that are produced in a melting process the ZsBeads are almost free of bubbles and pores. These properties increase their wear-resistance and prevent breaking. They are available in different fractions ranging from 0.6 mm to 1.8 mm.
Available standard qualities
Type | Fraction [mm] |
---|---|
ZsBeads 0.7 | 0.6 - 0.8 |
ZsBeads 0.9 | 0.8 - 1.0 |
ZsBeads 1.1 | 1.0 - 1.2 |
ZsBeads 1.3 | 1.2 - 1.4 |
ZsBeads 1.5 | 1.4 - 1.6 |
ZsBeads 1.7 | 1.6 - 1.8 |
Chemical composition
about (in weight %) | |
---|---|
ZrO2 | 64 |
SiO2 | 33 |
Others | 3 |
Mechanical properties
Density | 4.0 kg/l |
Bulk density | 2.5 kg/l |
Vickers hardness | 900 HV |