Yttrium-stabilized zirconium oxide grinding beads (Standard quality)

ZetaBeads® are spherical, yttrium-stabilized zirconium oxide grinding beads of a high density and hardness. In contrast to ZetaBeads® Plus and ZetaBeads® Nano their surface is not polished. ZetaBeads® are low-wear grinding beads that are used for the iron-free production of highquality products.

Available standard qualities

TypeFraction [mm]
ZetaBeads® 0.20.2 - 0.3
ZetaBeads® 0.30.3 - 0.4
ZetaBeads® 0.40.4 - 0.5
ZetaBeads® 0.50.5 - 0.6
ZetaBeads® 0.60.6 - 0.7
ZetaBeads® 0.80.7 - 0.9
ZetaBeads® 1.00.9 - 1.2
ZetaBeads® 1.31.2 - 1.5
ZetaBeads® 1.71.5 - 2.0
ZetaBeads® 2.22.0 - 2.5
ZetaBeads® 3.02.6 - 3.3

Chemical composition

about (in weight %) 
ZrO2 + HfO294
Y2O35
Others< 1

Mechanical properties

  
Densitiy6.0 kg/l
Bulk density3.6 kg/l
Young modulus> 200 GPa
Vickers hardness> 1100 HV

Request Product

We do not only promise quality, but also individual consulting. Let us start your project together.

Your Inquiry

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

you may also be interested in: