ZetaBeads® Plus are yttrium-stabilized high-end zirconium oxide grinding beads of a high density and hardness. In addition, the very good roundness and polished surface of the grinding beads contribute to an extremely high wearresistance with practically no product contamination. ZetaBeads® Plus grinding media are ideal for dispersion processes and real comminution of materials and products in the nano particle range.
Available standard qualities
Type | Fraction [mm] |
---|---|
ZetaBeads® Plus 0.07 | 0.07 - 0.12 |
ZetaBeads® Plus 0.1 | 0.1 - 0.2 |
ZetaBeads® Plus 0.2 | 0.2 - 0.3 |
ZetaBeads® Plus 0.3 | 0.3 - 0.4 |
ZetaBeads® Plus 0.4 | 0.4 - 0.5 |
ZetaBeads® Plus 0.5 | 0.5 - 0.6 |
Chemical composition
about (in weight %) | |
---|---|
ZrO2 + HfO2 | 94 |
Y2O3 | 5 |
Others | < 1 |
Mechanical properties
Densitiy | 6.0 kg/l |
Bulk density | 3.6 kg/l |
Young modulus | > 200 GPa |
Vickers hardness | > 1150 HV |