SteelBeads Micro are spherical cast steel grinding beads of tempered carbon steel. The fine-grained microstructure of the grinding beads give them a long lifetime and high breakage resistance. The SteelBeads Micro are available in a diameter range of 0.25 mm to 1.4 mm.
Available standard qualities
Type | Ø [mm] |
---|---|
SteelBeads Micro 0.25 | 0.25 |
SteelBeads Micro 0.5 | 0.5 |
SteelBeads Micro 1.0 | 1.0 |
SteelBeads Micro 1.2 | 1.2 |
SteelBeads Micro 1.4 | 1.4 |
Chemical composition
Element | weight % |
---|---|
C | 1 |
Mn | 0.9 |
P | - |
S | - |
Si | 0.5 |
Fe | Rest |
Mechanical properties
Densitiy | 7.6 kg/l |
Bulk density | 4.5 kg/l |