GlassBeads are bubble-free glass grinding beads with a density of 2.5 kg/l. They are especially recommended for wet grinding applications in the low to medium viscosity range. This is also true for applications for which the use of high-quality zirconium oxide grinding beads is no real alternative due to the high costs.
Available standard qualities
Type | Fraction [mm] |
---|---|
GlassBeads 0.5 | 0.4 - 0.6 |
GlassBeads 0.6 | 0.5 - 0.75 |
GlassBeads 0.9 | 0.75 - 1.0 |
GlassBeads 1.2 | 1.0 - 1.3 |
GlassBeads 1.5 | 1.25 - 1.65 |
GlassBeads 1.7 | 1.55 - 1.85 |
GlassBeads 1.9 | 1.7 - 2.1 |
Chemical composition
about (in weight %) | |
---|---|
SiO2 | 72.5 |
Na2O | 13 |
CaO | 9 |
MgO | 4 |
Al2O3 | < 0.6 |
Others | Rest |
Mechanical properties
Densitiy | 2.5 kg/l |
Bulk density | 1.5 kg/l |