Baterias

Anode and Cathode Materials
 

One option for the synthesis of cathode and anode materials is the so-called solid-state process. In this process route, the active material is created from the raw materials through a chemical transformation in suitable furnaces. Depending on the raw materials used, a wet grinding stage with dry pre-grinding processes can be required for the raw materials prior to the synthesis.

The CGS and s-Jet® fluidized bed jet mills can be used for the dry grinding. For the wet grinding, the Zeta®, Neos or Zeta® RS agitator bead mills are used, depending on the required target fineness. Synthesis via a furnace process can result in the formation of undesired agglomerates. In order to separate these, a dry dispersion with a CSM classifier mill is usually carried out after the synthesis furnace, without change of the original size and shape of primary particles.

Typical compounds for cathode materials are:
  • LCO (Lithium Cobalt Oxide, LiCoO2)
  • NCA (Lithium Nickel Cobalt Aluminum Oxide, LiNiCoAlO2)
  • NMC (Lithium Nickel Manganese Cobalt Oxide, Li[NiCoMn]O2)
  • LMO (Lithium Manganese Oxide, LiMn2O4)
  • LFP (Lithium Iron Phosphate, LiFePO4)
  • The conductor foil is usually made of aluminum
     
Some examples of active materials for anodes are:
  • Amorphous Carbon
  • Graphite
  • Lithium Titanate (LTO, Li4Ti5O12)
  • Metallic Anode Materials (Silicon, Tin)
  • The conductor foil is usually made of copper.

Contact Applications

We do not only promise quality, but also individual consulting. Let us start your project together.

Request information

Wet Grinding 

Products & Solutions in the field of Wet Grinding

Dry Grinding 

Products & Solutions in the field of Dry Grinding