CeraBeads are cerium-stabilized zirconium oxide grinding beads of a high density and hardness. They are suitable for different kinds of applications demanding an iron-free grinding process. CeraBeads simultaneously optimize your costs and grinding efficiency.
Available standard qualities
Type | Fraction [mm] |
---|---|
CeraBeads 0.4 | 0.4 - 0.6 |
CeraBeads 0.6 | 0.6 - 0.8 |
CeraBeads 1.0 | 0.9 - 1.1 |
CeraBeads 1.2 | 1.1 - 1.4 |
CeraBeads 1.4 | 1.4 - 1.6 |
CeraBeads 1.6 | 1.6 - 1.8 |
CeraBeads 1.8 | 1.8 - 2.0 |
CeraBeads 2.0 | 2.0 - 2.2 |
CeraBeads 2.6 | 2.5 - 2.8 |
CeraBeads 3.0 | 2.9 - 3.1 |
Chemical composition
about (in weight %) | |
---|---|
ZrO2 | 82 |
CeO2 | 16 |
Others | 2 |
Mechanical properties
Densitiy | 6.2 kg/l |
Bulk density | 3.8 kg/l |
Vickers hardness | > 1180 HV |