NETZSCH-Beads®

ZsBeads

Zirconium silicate grinding beads

ZsBeads are sintered zirconium silicate grinding beads with a high sphericity. In contrast to grinding beads that are produced in a melting process the ZsBeads are almost free of bubbles and pores. These properties increase their wear-resistance and prevent breaking. They are available in different fractions ranging from 0.6 mm to 1.8 mm.

Available standard qualities

TypeFraction [mm]
ZsBeads 0.70.6 - 0.8
ZsBeads 0.90.8 - 1.0
ZsBeads 1.11.0 - 1.2
ZsBeads 1.31.2 - 1.4
ZsBeads 1.51.4 - 1.6
ZsBeads 1.71.6 - 1.8

Chemical composition

about (in weight %) 
ZrO264
SiO233
Others3

Mechanical properties

  
Density4.0 kg/l
Bulk density2.5 kg/l
Vickers hardness900 HV

Request Product

We do not only promise quality, but also individual consulting. Let us start your project together.

Your Inquiry

Your Contact at NETZSCH

Any specific questions? Contact us for help. 

También podría estar interesado en: