Hardened steel grinding beads made of roller bearing steel

SteelBeads HQ are hardened grinding beads made of roller bearing steel with a very good roundness and smooth surface. The beads have a density of 7.85 kg/l and the diameters available range from 1.6 mm to 8.7 mm. This type of beads is mainly used for pasty printing ink applications.

Available standard qualities

TypeØ [mm]
SteelBeads HQ 1.61.6
SteelBeads HQ 22.0
SteelBeads HQ 33.0
SteelBeads HQ 44.0
SteelBeads HQ 55.0
SteelBeads HQ 66.0
SteelBeads HQ 88.0
SteelBeads HQ 98.7

Chemical composition

Elementweight %
C1
Mn0.3
Cr1.5
Mo0.1
P-
S-
Si0.2
Cu0.3
Al-
FeRest

Mechanical properties

  
Densitiy7.85 kg/l
Bulk density4.8 kg/l
Vickers hardness740 - 900 HV

Request Product

We do not only promise quality, but also individual consulting. Let us start your project together.

Your Inquiry

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

También podría estar interesado en: