ZetaBeads® Nano are made of yttrium-stabilized, high-purity zirconium oxide powder. Thanks to their high density and extreme hardness product contamination is avoided. With diameters ranging from 30 μm to 200 μm ZetaBeads® Nano are particularly suitable for ispersion and wet grinding of high-tech products down to the lower nanometer range.
Available standard qualities
Type | Ø [mm] |
---|---|
ZetaBeads® Nano 0.03 | 0.03 |
ZetaBeads® Nano 0.05 | 0.05 |
ZetaBeads® Nano 0.1 | 0.1 |
ZetaBeads® Nano 0.2 | 0.2 |
Chemical composition
about (in weight %) | |
---|---|
ZrO2 + HfO2 | 95 |
Y2O3 | 5 |
Mechanical properties
Densitiy | 6.0 kg/l |
Bulk density | 3.6 kg/l |
Young modulus | > 200 GPa |
Vickers hardness | > 1200 HV |