NETZSCH-Beads®

ZetaBeads® Plus

Yttrium-stabilized zirconium oxide grinding beads (High-end quality)

ZetaBeads®®Plus are yttrium-stabilized high-end zirconium oxide grinding beads of a high density and hardness. In addition, the very good roundness and polished surface of the grinding beads contribute to an extremely high wearresistance with practically no product contamination. ZetaBeads®®Plus grinding media are ideal for dispersion processes and real comminution of materials and products in the nano particle range.

Available standard qualities

TypeFraction [mm]
ZetaBeads®®Plus 0.070.07 - 0.12
ZetaBeads®®Plus 0.10.1 - 0.2
ZetaBeads®®Plus 0.20.2 - 0.3
ZetaBeads®®Plus 0.30.3 - 0.4
ZetaBeads®®Plus 0.40.4 - 0.5
ZetaBeads®®Plus 0.50.5 - 0.6

Chemical composition

about (in weight %) 
ZrO2 + HfO294
Y2O35
Others< 1

Mechanical properties

  
Densitiy6.0 kg/l
Bulk density3.6 kg/l
Young modulus> 200 GPa
Vickers hardness> 1150 HV

Request Product

We do not only promise quality, but also individual consulting. Let us start your project together.

Your Inquiry

Your Service Contact at NETZSCH

Any specific questions? Contact us for help. 

you may also be interested in: